JOURNAL OF LIGHT INDUSTRY

CN 41-1437/TS  ISSN 2096-1553

膨胀蛭石偶联的羟基封端硅橡胶及其阻燃性能优化研究

郭东杰 王彦辉 白宝丰 闫春绵 史波 方少明

郭东杰, 王彦辉, 白宝丰, 等. 膨胀蛭石偶联的羟基封端硅橡胶及其阻燃性能优化研究[J]. 轻工学报, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003
引用本文: 郭东杰, 王彦辉, 白宝丰, 等. 膨胀蛭石偶联的羟基封端硅橡胶及其阻燃性能优化研究[J]. 轻工学报, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003
GUO Dong-jie, WANG Yan-hui, BAI Bao-feng, et al. Hydroxyl terminated poly(dimethylsiloxane) crosslinked by expanded vermiculite and its flame retardant performance optimization[J]. Journal of Light Industry, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003
Citation: GUO Dong-jie, WANG Yan-hui, BAI Bao-feng, et al. Hydroxyl terminated poly(dimethylsiloxane) crosslinked by expanded vermiculite and its flame retardant performance optimization[J]. Journal of Light Industry, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003

膨胀蛭石偶联的羟基封端硅橡胶及其阻燃性能优化研究

  • 基金项目: 教育部"长江学者和创新团队发展计划"创新团队(IRT1187)
    973国家重点基础研究发展计划(2014CB239600)
    河南省重点攻关项目(132102210240)

  • 中图分类号: TQ333.93

Hydroxyl terminated poly(dimethylsiloxane) crosslinked by expanded vermiculite and its flame retardant performance optimization

  • Received Date: 2015-10-27
    Available Online: 2016-03-15

    CLC number: TQ333.93

  • 摘要: 以羟基封端硅橡胶为主体、高温膨胀蛭石(EV)为添加剂、四乙氧基硅为偶联剂,经两步缩合反应制备了蛭石/硅橡胶复合弹性体(EV-PDMS),并对其阻燃性能进行了研究.经分别用全反射衰减红外光谱、水接触角、扫描电子显微镜对制备物进行测试,结果表明:膨胀蛭石的片状晶体均匀地分散于硅橡胶的内部,它们之间形成了稳定的Si-O-Si共价键,掺杂后的EV-PDMS弹性体表面维持了高度的憎水性能.力学性能测试表明:60份EV掺杂后,拉伸强度、杨氏模量、邵氏硬度分别增加至添加前空白PDMS弹性体的4.50倍、1.97倍、2.17倍.燃烧实验表明:添加5份的十溴联苯醚和5份的氢氧化铝,蛭石/硅橡胶弹性体的阻燃性能可达到FV-0级,极限氧指数可达69.5%.
    1. [1]

      GUO D J,XIAO S J,LIU H B,et al.Diffusion of hydrosilanes from the control layer to the vinylsilane-rich flow membrane during the fabrication of microfluidic chips[J].Langmuir,2005,21(23):10487.

    2. [2]

      JI C T,WANG J H,SONG J N,et al.Development of ceramificable silicone rubber for flame retardancy and fire-resisting materials[J].Journal of functional materials,2015,46(4):04001.

    3. [3]

      方少明,程瑜,百宝丰,等.缩合型硅橡胶发泡配方优化及保温性能研究[J].郑州轻工业学院学报(自然科学版),2014,29(2):1.

    4. [4]

      LAI L Q,QIAN H H,SU Z T,et al.Study on mechanical properties and flammability of montmorillonite/silicone rubber composites[J].Silicone materials,2008,22(1):24.

    5. [5]

      GUO J H,LUO K,ZENG X R.Property study of retardant silicone rubber filled by aluminium hydroxide[J].China rubber industry,2007(8):471.

    6. [6]

      ZHAN X G.Study of flame-retardant HTV silicone rubber with aluminum hydroxide[J].Silicone materials,2010,24(2):92.

    7. [7]

      YANG L,HU Y,LU H D,et al.Morphology,thermal,and mechanical properties of flame-retardant silicone rubber/montmorillonite nanocomposites[J].Journal of applied polymer science,2006,99:3275.

    8. [8]

      XI Y G,PENG T J.Preparation and characterization of expanded vermiculite/gypsum thermal insulation composites[J].Acta materiae compositae sinica,2011,28(5):156.

    9. [9]

      GUO D J,HAN H M,WANG J,et al.Surface-hydrophilic and protein-resistant silicone elastomers prepared by hydrosilylation of vinyl poly(ethylene glycol) on drosilanes-poly (dimethylsiloxane) surfaces[J].Colloids surface A:physcochemical and engineering aspects,2007,308(1/3):129.

    10. [10]

      TANG Y J,JIANG X H,XUE G X,et al.Layer-by-layer self-assembly of CS/APAM on the surface of recycled fiber[J].Journal of functional materials,2010,41(10):1820.

    11. [11]

      GUO D J,ABDULAGATOV A I,ROURKE D M,et al.GaN nanowire functionalized with atomic layer deposition techniques for enhanced immobilization of biomolecules[J].Langmuir,2010,26(23):18382.

    12. [12]

      GUO D J,FU S J,TAN W,et al.A highly porous nafion membrane templated from polyoxometalates-based supramolecule composite for IPMC actuator[J].Journal of materials chemistry,2010,20:10159.

    13. [13]

      YU K H,DENG J F,WU M L,et al.The effects of silane coupling agents on the EPDM/MVQ[J].Materials review,2011,25(17):421.

    14. [14]

      ZHAO H X,SHI Y G,CHEN Y G,et al.Overview of oversea research on modification and performance evaluations of silicone rubber[J].Materials review,2013,27(11):57.

  • 加载中
计量
  • PDF下载量:  99
  • 文章访问数:  8648
  • 引证文献数: 0
文章相关
  • 收稿日期:  2015-10-27
  • 刊出日期:  2016-03-15
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索
郭东杰, 王彦辉, 白宝丰, 等. 膨胀蛭石偶联的羟基封端硅橡胶及其阻燃性能优化研究[J]. 轻工学报, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003
引用本文: 郭东杰, 王彦辉, 白宝丰, 等. 膨胀蛭石偶联的羟基封端硅橡胶及其阻燃性能优化研究[J]. 轻工学报, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003
GUO Dong-jie, WANG Yan-hui, BAI Bao-feng, et al. Hydroxyl terminated poly(dimethylsiloxane) crosslinked by expanded vermiculite and its flame retardant performance optimization[J]. Journal of Light Industry, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003
Citation: GUO Dong-jie, WANG Yan-hui, BAI Bao-feng, et al. Hydroxyl terminated poly(dimethylsiloxane) crosslinked by expanded vermiculite and its flame retardant performance optimization[J]. Journal of Light Industry, 2016, 31(2): 21-28. doi: 10.3969/j.issn.2096-1553.2016.2.003

膨胀蛭石偶联的羟基封端硅橡胶及其阻燃性能优化研究

  • 郑州轻工业学院材料与化学工程学院, 河南郑州 450001;
  • 南京航空航天大学能源与动力学院, 江苏南京 210096
基金项目:  教育部"长江学者和创新团队发展计划"创新团队(IRT1187)973国家重点基础研究发展计划(2014CB239600)河南省重点攻关项目(132102210240)

摘要: 以羟基封端硅橡胶为主体、高温膨胀蛭石(EV)为添加剂、四乙氧基硅为偶联剂,经两步缩合反应制备了蛭石/硅橡胶复合弹性体(EV-PDMS),并对其阻燃性能进行了研究.经分别用全反射衰减红外光谱、水接触角、扫描电子显微镜对制备物进行测试,结果表明:膨胀蛭石的片状晶体均匀地分散于硅橡胶的内部,它们之间形成了稳定的Si-O-Si共价键,掺杂后的EV-PDMS弹性体表面维持了高度的憎水性能.力学性能测试表明:60份EV掺杂后,拉伸强度、杨氏模量、邵氏硬度分别增加至添加前空白PDMS弹性体的4.50倍、1.97倍、2.17倍.燃烧实验表明:添加5份的十溴联苯醚和5份的氢氧化铝,蛭石/硅橡胶弹性体的阻燃性能可达到FV-0级,极限氧指数可达69.5%.